Direct Answer: an inspection on care and cleaning only decides one thing, whether the lot matches the retained reference piece on the measurements written down before production. AQL tables decide how many pieces to pull; they do not decide what a piece is supposed to be. Write the spec first, then sample against it, and the argument after delivery becomes arithmetic.
The plan below is the sampling we apply on a 300-piece order. Pull the care and cleanings before the trays are packed, not after, because a tray that has been wrapped is a tray nobody wants to unwrap.
| Lot size | Sample | Critical | Major | Minor |
|---|---|---|---|---|
| 50 to 150 pieces | 13 pieces | Zero | 2 | 3 |
| 151 to 500 pieces | 32 pieces | Zero | 3 | 5 |
| 501 to 1,200 pieces | 50 pieces | Zero | 5 | 7 |
| Over 1,200 pieces | 80 pieces | Zero | 7 | 10 |
A critical defect is stone loss, a broken prong, a clasp that opens under load, or metal that fails a nickel or lead screen. One piece stops the lot regardless of the lot size, because one piece is enough to generate the return, the detail a 300-piece run of care and cleaning is judged on.
Six stations sound like six costs. In practice the first three remove the reasons for the last three to reject anything, and the whole sequence adds a few minutes per tray rather than per piece, a detail that decides the reorder on care and cleaning at USD 8-42.
Nothing here needs a laboratory. A loupe, a gauge, a balance and a written sheet carry most of the quality a care and cleaning buyer is paying for, which is why the protocol travels with the trays.
A station without a signature is a station that did not happen. Ours carries the inspector's initials per lot, and the sheet ships in the carton so a claim can be argued from paper, which on a 300-piece run of care and cleaning is the number the order carries.

| Defect | Class | Likely cause | Fix at source |
|---|---|---|---|
| ('tarnish in transit', 'Silver that ships without an anti-tarnish strip browns in a humid container. The strip costs 3 cents and removes the most common arrival complaint.') | Major | Bench or spec gap | Gauge per size and a retained reference piece |
| ('rhodium adhesion', 'A silver surface plated without a palladium strike layer blisters in wear. The strike layer is invisible and essential.') | Major | Plating or casting prep | Porosity check before the plating bath |
| ('weight shortfall', 'A 2.1 g ring shipped at 1.85 g passes a casual check and fails a scale. Publish the weighed average per SKU.') | Critical or major | Component source | Incoming check on the component lot |
| Colour drift against the master | Major | Stone batching | Matched lot per tray, master stone on the bench |
| Sizing drift across the run | Major | Gauge not used | Go/no-go gauge on every size |
| Packing list mismatch | Minor to major | Dock reconciliation | Carton count signed before sealing |
Every row has a source upstream of the defect. Fixing the care and cleaning is a cost; fixing the row is a saving, and the difference is whether the cause is written down.
The first three rows account for most claims on care and cleaning. They are also the three that a bench check catches before packing, which is why the sequence matters more than the sample size.
A defect taxonomy is only useful if the words match across the order, the inspection and the claim. Ours uses the six terms above on the quote, the QC sheet and the credit note, the detail a 300-piece run of care and cleaning is judged on.
One critical defect stops the lot and triggers a hundred percent check of the affected tray before anything ships. The buyer does not receive a percentage with a note attached; the tray is either reworked or held, which on a 300-piece run of care and cleaning is the number the order carries.
A major defect rate above the plan triggers a second sample on the same lot before a decision. The second sample decides whether the cause is the run or the tray, and both outcomes are written on the sheet the same day, the detail a 300-piece run of care and cleaning is judged on.
A rejected tray is settled against the retained reference piece inside the same order cycle. If the difference shows on our retained piece we replace or credit; if it appeared in transit we split the assay cost and file with the carrier, and that split is on the order before the deposit clears, a detail that decides the reorder on care and cleaning at USD 8-42.
Minor defects inside the plan ship with the count stated on the packing list, so the buyer's receiving team knows what to expect rather than discovering it. Stating a minor defect is cheaper than hiding one, the same figure we quote on care and cleaning at USD 8-42.
The rule has to be signed before the run, because after the run it is a negotiation and the party holding the care and cleaning has the leverage. Writing it into the purchase order is the whole protection.
Buyers sometimes ask for a zero-defect clause. We quote it, and we quote the inspection cost that makes it possible, because zero without a hundred percent check is a promise rather than a process, a detail that decides the reorder on care and cleaning at USD 8-42.
A claim handled in the same cycle costs a credit note. A claim handled after the season costs the relationship, which is the more expensive of the two, the same figure we quote on care and cleaning at USD 8-42.
A third-party inspector adds independence, which matters when the factory is new to you and the order is large. It does not add specification: the inspector checks against the sheet you supply, so a vague sheet produces a vague report with a logo on it, a detail that decides the reorder on care and cleaning at USD 8-42.
The gap in most third-party reports is the retained reference. An inspector can measure a care and cleaning, but it cannot tell you whether the colour matches the master you approved, because it never saw the master. Send the reference piece with the inspection request.
Pay for an inspector on the first order above a few hundred pieces and on any order from a new factory. After two clean lots with the same spec, the money is better spent on your own receiving check and a gauge, which on a 300-piece run of care and cleaning is the number the order carries.
AQL 1.0 for major and 2.5 for minor on the lots above 150 pieces, with zero acceptance on critical defects. Below 150 pieces the lot is small enough that a hundred percent check on the care and cleaning costs less than a sampling argument.
32 pieces on a 300-piece run, pulled across trays rather than from one. Every size in the lot gets a gauge pass regardless of the sample, because drift is a run property and not a care and cleaning property.
Yes. We schedule it, provide the trays and the sheet, and hold production until the report lands. Inspectors who arrive without the retained reference usually produce a report about appearance rather than about specification, the detail a 300-piece run of care and cleaning is judged on.
Stone loss, a prong that will not hold under load, a clasp that opens, or metal that fails a nickel or lead screen. One occurrence stops the lot; the others are counted against the plan, a detail that decides the reorder on care and cleaning at USD 8-42.
Both, at different stations. Porosity is checked before the plating bath, and plating thickness and colour are checked after it. An inspection that only happens at the end cannot tell you which of the two failed, the same figure we quote on care and cleaning at USD 8-42.
Send the lot size and the defect history from your last order, and the reply comes back with the sampling plan, the six stations and the reject rule written for that lot rather than for a generic one, which on a 300-piece run of care and cleaning is the number the order carries.
HOLYCOME is the export arm of Wuzhou HengliLai Jewelry Co., Ltd., a Wuzhou, Guangxi plant that has shipped since 2009 and produces about 60,000 pieces a month, care and cleaning included. Export paperwork, the certificate pack and the packing list are prepared in-house, which is why the documents quoted on the order are the ones that travel with the carton. Reach the desk at service@holycome.com or WhatsApp +86 18078079070.
Related reading: Care & Cleaning Supplier: The Scorecard We Run on Our Own Vendors - HOLYCOME Sizing Guide Trade Show Sample: What the Quote Actually Covers - HOLYCOME
Wuzhou HengliLai Jewelry Co., Ltd. - Professional gemstone and jewelry manufacturer in Wuzhou, China. OEM/ODM services, factory-direct pricing, low MOQ.
Contact on WhatsApp service@holycome.comWritten by the Holycome manufacturing & quality team. Every figure and claim in this article comes from our own production floor in Wuzhou, China — in-house casting, stone setting and a three-pass quality inspection we have run since 2008.
Materials are tested for nickel, lead and cadmium release by SGS and CTT International; moissanite centre stones ship with their GRA warranty card and report. We also hold an independent SMETA / Sedex ethical-trade audit and a Hong Kong Customs AML registration.
Reviewed for accuracy by our quality team before publication. Last updated .